Delignification through the Mini-O process presents itself
as much more inexpensive alternative when compared with the
conventional delignification with Oxygen. This is due to the
fact that the Mini-O process needs substantially smaller investment
in new equipment such as: MC pump, mixer and reactor or retention
tube.
|
|
| |
|
| |
 |
| |
| Mini-delignification with Oxygen (Mini-O) |
|
| |
|
| |
|
Mini-O operational conditions are less intense then the conventional
Oxygen delignification, therefore its benefits are similar
to the ones seen in the conventional process, although with
proportionally lower values. The Mini-O process offers many
interesting benefits to plants with no capital for high investments
|
|
| |
|
| |
|
Conventional |
Mini-O |
|
| Investment
(MM US$) |
20
|
1-
3 |
|
|
|
|
|
| Delignification
(%) |
|
|
|
| Hardwood |
35
- 40 |
20
- 25 |
|
| Softwood |
40
- 50 |
25
- 30 |
|
|
|
|
|
| Operational
Parameters |
|
|
|
| Temperature
(° C) |
100
- 110 |
80
- 90 |
|
| Retention
Time (min) |
60
- 90 |
20
- 30 |
|
| Pressure
(kgf/cm²) |
5,0
- 7,0 |
3,5
- 7,0 |
|
| Oxygen
( % odp) |
2,0 |
1,0
- 1,5 |
|
| Álkali
(% odp) |
2,0 |
1,0
- 2,0 |
|
|
| |
|
| |
Would you like more information? Contact
us |
|
|
|
|
|